Click Here for 5% Off Your First Aladdin Purchase!

Poly(3,4-ethylenedioxythiophene), bis-poly(ethyleneglycol), lauryl terminated - 0.7wt. % (dispersion in nitromethane), high purity

  • 0.7wt. % (dispersion in nitromethane)
Item Number
P466049
Grouped product items
SKUSizeAvailabilityPrice Qty
P466049-25g
25g
Available within 8-12 weeks(?)
Production requires sourcing of materials. We appreciate your patience and understanding.
$675.90

Basic Description

Specifications & Purity0.7wt. % (dispersion in nitromethane)
Legal InformationAedotron is a trademark of TDA Research, Inc.
Product Description

Description

Please follow this link forAedotron/Oligotron selection guide table.Aedotron™polymers are solvent-dispersable forms of PEDOT. These are copolymers of doped PEDOT and a flexible, soluble polymer such as poly(ethylene glycol) (PEG). These colloidal dispersions are stabilized by the highly solvated PEG chains which sterically limit the aggregation of the PEDOT blocks. Aedotron polymers are neither acidic nor corrosive, it easily disperses in polar aprotic solvents. Aedotron™C3-NM is a triblock copolymer.Nitromethane dispersions can be used to cast thin films on glass, ITO, silicon wafers and many polymeric substrates. Compatibility of the polymeric substrate with nitromethane should be tested in each case. Coat the substrate with a "pool" of the nitromethane dispersion. Thin transparent films are typically spun at 1000 RPM or higher speeds, but more conducting films can be obtained at lower speeds. A single layer spun at 1000 RPM is typically 75 nm thick.Conducting polymer dispersion suitable for making conducting films, anti-static layers and transparent electrodes for electroluminescent lamps.

Certificates

Certificate of Analysis(COA)

Enter Lot Number to search for COA:

Chemical and Physical Properties

SensitivityPlease store this product at room temperature (do not freeze or refrigerate). If there is a slight precipitation in the product, it is a normal phenomenon. Before use, please stir, sonicate, and filter. Glass wool can be filled at the front end of the pip