Click Here for 5% Off Your First Aladdin Purchase!

Silicon monoxide - 99.99% metals basis, −325 mesh, high purity , CAS No.10097-28-6

  • PrimorTrace™
  • ≥99.99% metals basis
  • >325 mesh
Item Number
S431223
Grouped product items
SKUSizeAvailabilityPrice Qty
S431223-10g
10g
Available within 8-12 weeks(?)
Production requires sourcing of materials. We appreciate your patience and understanding.
$39.90
S431223-50g
50g
Available within 8-12 weeks(?)
Production requires sourcing of materials. We appreciate your patience and understanding.
$149.90
S431223-250g
250g
Available within 8-12 weeks(?)
Production requires sourcing of materials. We appreciate your patience and understanding.
$599.90
View related series
Oxides & Ceramics

Basic Description

SynonymsSilicon monoxide|10097-28-6|Silylene, oxo-|Silicon(II) oxide|oxosilicon|EINECS 233-232-8|13779-62-9|MFCD00151536|1OQN9CBG7L|SiO|oxosilylene|Silicon oxide (SiO)|UNII-1OQN9CBG7L|oxidosilicon|silanone|Silanoxide|Oxosilane|silicon monooxide|SILICONMONOXIDE|Si
Specifications & Purity99.99% metals basis, −325 mesh
GradePrimorTrace™

Names and Identifiers

IUPAC Name oxosilicon
INCHI InChI=1S/OSi/c1-2
InChi Key LIVNPJMFVYWSIS-UHFFFAOYSA-N
Canonical SMILES O=[Si]
Isomeric SMILES O=[Si]
WGK Germany 3
PubChem CID 66241
Molecular Weight 44.08

Certificates

Certificate of Analysis(COA)

Enter Lot Number to search for COA:

To view the certificate results,please click on a Lot number.For Lot numbers from past orders,please use our order status section

6 results found

Lot NumberCertificate TypeDateItem
H2413357Certificate of AnalysisJul 26, 2024 S431223
H2413358Certificate of AnalysisJul 26, 2024 S431223
H2413359Certificate of AnalysisJul 26, 2024 S431223
H2413360Certificate of AnalysisJul 26, 2024 S431223
H2413361Certificate of AnalysisJul 26, 2024 S431223
H2413362Certificate of AnalysisJul 26, 2024 S431223

Chemical and Physical Properties

Boil Point(°C)1880°C
Melt Point(°C)>1702°C

Safety and Hazards(GHS)

Pictogram(s) GHS07
Signal Warning
Hazard Statements

H315:Causes skin irritation

H319:Causes serious eye irritation

H335:May cause respiratory irritation

Precautionary Statements

P261:Avoid breathing dust/fume/gas/mist/vapors/spray.

P305+P351+P338:IF IN EYES: Rinse cautiously with water for several minutes. Remove contact lenses if present and easy to do - continue rinsing.

P280:Wear protective gloves/protective clothing/eye protection/face protection.

P302+P352:IF ON SKIN: wash with plenty of water.

P321:Specific treatment (see ... on this label).

P405:Store locked up.

P501:Dispose of contents/container to ...

P264:Wash hands [and …] thoroughly after handling.

P271:Use only outdoors or in a well-ventilated area.

P304+P340:IF INHALED: Remove person to fresh air and keep comfortable for breathing.

P403+P233:Store in a well-ventilated place. Keep container tightly closed.

P362+P364:Take off contaminated clothing and wash it before reuse.

P264+P265:Wash hands [and …] thoroughly after handling. Do not touch eyes.

P337+P317:If eye irritation persists: Get medical help.

P332+P317:If skin irritation occurs: Get medical help.

P319:Get medical help if you feel unwell.

WGK Germany 3

Related Documents

References

1. Jürgen Becker,Günther Grün,Ralf Seemann,Hubert Mantz,Karin Jacobs,Klaus R Mecke,Ralf Blossey.  (2003-03-26)  Complex dewetting scenarios captured by thin-film models..  Nature materials,  ((1)): (59-63).  [PMID:12652675]
2. F C Yuan,G Z Ran,Y Chen,B R Zhang,Y P Qiao,J S Fu,G G Qin,Z C Ma,W H Zong.  (2003-09-10)  [Photoluminescence from Er-doped silicon-rich silicon oxide film and Er-doped silicon-rich silicon nitride film and its annealing behavior]..  Guang pu xue yu guang pu fen xi = Guang pu,  21  ((6)): (763-765).  [PMID:12958888]
3. Maggie Paulose,Oomman K Varghese,Craig A Grimes.  (2003-11-06)  Synthesis of gold-silica composite nanowires through solid-liquid-solid phase growth..  Journal of nanoscience and nanotechnology,  ((4)): (341-346).  [PMID:14598450]
4. C S Tang,P Schmutz,S Petronis,M Textor,B Keller,J Vörös.  (2005-06-25)  Locally Addressable Electrochemical Patterning Technique (LAEPT) applied to poly(L-lysine)-graft-poly(ethylene glycol) adlayers on titanium and silicon oxide surfaces..  Biotechnology and bioengineering,  91  ((3)): (285-295).  [PMID:15977251]
5. Michael J R Previte,Chris D Geddes.  (2007-04-04)  Microwave-triggered chemiluminescence with planar geometrical aluminum substrates: theory, simulation and experiment..  Journal of fluorescence,  17  ((3)): (279-287).  [PMID:17404821]
6. Toshiaki Suzuki,Yoshitaka Hamashima,Mikiko Sodeoka.  (2007-06-15)  Asymmetric fluorination of alpha-aryl acetic acid derivatives with the catalytic system NiCl2-Binap/R3SiOTf/2,6-lutidine..  Angewandte Chemie (International ed. in English),  46  ((28)): (5435-5439).  [PMID:17568468]
7. Etienne Garand,Daniel Goebbert,Gabriele Santambrogio,Ewald Janssens,Peter Lievens,Gerard Meijer,Daniel M Neumark,Knut R Asmis.  (2008-03-11)  Vibrational spectra of small silicon monoxide cluster cations measured by infrared multiple photon dissociation spectroscopy..  Physical chemistry chemical physics : PCCP,  10  ((11)): (1502-1506).  [PMID:18327305]
8. Frank Welle,Roland Franz.  (2008-05-20)  SiOx layer as functional barrier in polyethylene terephthalate (PET) bottles against potential contaminants from post-consumer recycled PET..  Food additives & contaminants. Part A, Chemistry, analysis, control, exposure & risk assessment,  25  ((6)): (788-794).  [PMID:18484307]
9. Chih-Wei Hsu,Huei-Ru Liou,Wei-Fang Su,Leeyih Wang.  (2008-06-03)  Self-assembled monolayers of 2-(thienyl)hexylphosphonic acid on native oxide surface of silicon fabricated by air-liquid interface-assisted method..  Journal of colloid and interface science,  324  ((1-2)): (236-239).  [PMID:18513736]
10. Vishva Ray,Ramkumar Subramanian,Pradeep Bhadrachalam,Liang-Chieh Ma,Choong-Un Kim,Seong Jin Koh.  (2008-10-08)  CMOS-compatible fabrication of room-temperature single-electron devices..  Nature nanotechnology,  ((10)): (603-608).  [PMID:18838999]
11. Simon Grabowsky,Maxie F Hesse,Carsten Paulmann,Peter Luger,Jens Beckmann.  (2009-04-22)  How to make the ionic Si-O bond more covalent and the Si-O-Si linkage a better acceptor for hydrogen bonding..  Inorganic chemistry,  48  ((10)): (4384-4393).  [PMID:19379009]
12. Norman A Lapin,Yves J Chabal.  (2009-06-06)  Infrared characterization of biotinylated silicon oxide surfaces, surface stability, and specific attachment of streptavidin..  The journal of physical chemistry. B,  113  ((25)): (8776-8783).  [PMID:19489542]
13. Chang-Ying Xue,Kun-Lin Yang.  (2010-01-12)  One-step UV lithography for activation of inert hydrocarbon monolayers and preparation of protein micropatterns..  Journal of colloid and interface science,  344  ((1)): (48-53).  [PMID:20060543]
14. Jana Lokajová,Jaana Laine,Esa Puukilainen,Mikko Ritala,Juha M Holopainen,Susanne K Wiedmer.  (2010-04-02)  Liposomes for entrapping local anesthetics: a liposome electrokinetic chromatographic study..  Electrophoresis,  31  ((9)): (1540-1549).  [PMID:20358540]
15. Nam-Joon Cho,Curtis W Frank,Bengt Kasemo,Fredrik Höök.  (2010-06-12)  Quartz crystal microbalance with dissipation monitoring of supported lipid bilayers on various substrates..  Nature protocols,  ((6)): (1096-1106).  [PMID:20539285]
16. Deheng Shi,Wentao Li,Jinfeng Sun,Zunlue Zhu.  (2011-12-16)  MRCI study on the spectroscopic parameters and molecular constants of the X1Σ+, a3Σ+, A1Π and C1Σ- electronic states of the SiO molecule..  Spectrochimica acta. Part A, Molecular and biomolecular spectroscopy,  87  (96-105).  [PMID:22169566]
17. Hongwei Ma,Dejin Li,Xia Sheng,Bin Zhao,Ashutosh Chilkoti.  (2006-04-06)  Protein-resistant polymer coatings on silicon oxide by surface-initiated atom transfer radical polymerization..  Langmuir : the ACS journal of surfaces and colloids,  22  ((8)): (3751-3756).  [PMID:16584252]
18. Arthur C Reber,Penee A Clayborne,J Ulises Reveles,Shiv N Khanna,A W Castleman,Ashraf Ali.  (2006-06-15)  Silicon oxide nanoparticles reveal the origin of silicate grains in circumstellar environments..  Nano letters,  ((6)): (1190-1195).  [PMID:16771578]
19. A Butterwick,P Huie,B W Jones,R E Marc,M Marmor,D Palanker.  (2008-10-29)  Effect of shape and coating of a subretinal prosthesis on its integration with the retina..  Experimental eye research,  88  ((1)): (22-29).  [PMID:18955050]
20. Elisabeth Galopin,Gaelle Piret,Sabine Szunerits,Yannick Lequette,Christine Faille,Rabah Boukherroub.  (2009-11-07)  Selective adhesion of Bacillus cereus spores on heterogeneously wetted silicon nanowires..  Langmuir : the ACS journal of surfaces and colloids,  26  ((5)): (3479-3484).  [PMID:19891454]
21. Parijat Bhatnagar,George G Malliaras,Il Kim,Carl A Batt.  (2010-05-04)  Multiplexed protein patterns on a photosensitive hydrophilic polymer matrix..  Advanced materials (Deerfield Beach, Fla.),  22  ((11)): (1242-1246).  [PMID:20437512]
22. Taizo Kobayashi,Kazunori Shimizu,Yoshihiro Kaizuma,Satoshi Konishi.  (2010-12-04)  Novel combination of hydrophilic/hydrophobic surface for large wettability difference and its application to liquid manipulation..  Lab on a chip,  11  ((4)): (639-644).  [PMID:21127789]
23. Wei-Hsun Yeh,Joseph W Petefish,Andrew C Hillier.  (2011-06-22)  Diffraction-based tracking of surface plasmon resonance enhanced transmission through a gold-coated grating..  Analytical chemistry,  83  ((15)): (6047-6053).  [PMID:21688830]
24. Peter Cuony,Duncan T L Alexander,Ivan Perez-Wurfl,Matthieu Despeisse,Gregory Bugnon,Mathieu Boccard,Thomas Söderström,Aïcha Hessler-Wyser,Cécile Hébert,Christophe Ballif.  (2012-02-01)  Silicon filaments in silicon oxide for next-generation photovoltaics..  Advanced materials (Deerfield Beach, Fla.),  24  ((9)): (1182-1186).  [PMID:22290779]
25. D Y Ju,P Bian,T Kumazawa,M Nakano,H Matsuura,K Umetani,T Komdo,Y Uozumi,K Makino,N Noda,K Koide,M Akutsu,K Masuyama.  (2012-03-10)  Drug delivery observation of hydrophobe ferrofluid and magnetite nanoparticals by SPring-8 synchrotron radiation..  Journal of nanoscience and nanotechnology,  11  ((10)): (8738-8743).  [PMID:22400252]

Solution Calculators